I. Types of coating equipment industry
1, automobile machinery and equipment coating equipment
For example: dust-free spray booth, dust-free spray booth, automobile coating line, automatic spray painting, automobile electrophoretic coating line, rain test, etc.
2, mobile phone shell, electrical shell coating equipment
For example: automatic UV spraying line. Electrostatic coating line.
3, wooden furniture, handicrafts, floor, wallboard coating equipment
For example: primer sander, roller coater, automatic painting line, electrostatic coating line, NC paint roller coating line, UV paint roller coating line, positive pressure clean room, dust-free baking room, water curtain painting table, hanging wire, vacuum polishing table, dust remover, curtain shower belt conveyor line, etc.
4. Steel furniture. Steel art handicraft painting equipment
For example: pretreatment equipment, electrostatic coating line, etc.
5、通用涂料工業設備:
比如:線條畫機、木門往復畫機、五軸多軸直線外掛運動畫機、四軸六軸繪畫機器人。
二、噴涂操作的常見問題及解決方法:
1.現象:起球
原因:作業現場不干凈,灰塵混入油漆中;涂料混合后放置過久,涂料和固化劑產生了共聚顆粒;噴槍出油量太小,氣壓太高,使油漆霧化不良或噴槍離物體表面太近。
解決方法:清理噴漆室,蓋好油漆桶;油漆攪拌均勻,不宜放置過久;調整噴槍,使其處于最佳工作狀態,并確保槍口距離物體表面20-50厘米。
2.現象:垂直流動
原因:稀釋劑過多使油漆粘度過低,失去粘性;出油量太大、離物體表面太近或噴涂操作太慢;每次噴油太多太稠或再噴油間隔太短;物體表面凹凸不平,特別是流線形狀容易產生垂直流動。
解決方法:按要求混合;控制出油量,保證油漆分離,提高噴槍運行速度;每次噴不要太厚,最好分兩次掌握間隔涂刷時間;控制出油量,降低漆膜厚度;根據使用說明混合
3.現象:橘皮
原因:固化劑過多使漆膜干燥過快,反應劇烈;噴涂氣壓過高使漆膜起皺以致無法流平;作業現場溫度太高,為什么漆膜要暴力?
解決方法:按說明混合;調節氣壓,不要太大;注意現場溫度,可加入慢干稀釋劑抑制干燥速度。
4.現象:變白
原因:作業現場溫濕度較高,漆膜反應劇烈,可能與空氣中的水分結合產生泛白現象;固化劑過量,一次噴太多太厚。
解決方法:注意現場濕度,加防水白水,防止泛白;比例調制,一噴不宜過濃。
5.現象:起泡
原固體:漆膜上混有水的壓縮空氣,作業現場溫度高,油漆干燥過快;物體表面含水量高,空氣濕度大;一噴太濃。
解決方法:油水分離,注意排水;加入慢干稀釋劑;清潔表面,用白水涂漆;一次不宜過濃。
6.現象:收縮
原因:底漆或中間漆在涂面漆前沒有完全干燥。
解決方案;根據每個掃描槍涂層的推薦厚度進行噴涂。
7.現象:起皺
原因:干燥時間太短或漆膜太厚;底漆或膩子中固化劑選擇不當;底漆膩子不完整;噴面漆時,一槍走得太厚,內部深層劑沒有及時揮發,所以外干內不干。
解決方法:在每道涂層之間給予足夠的干燥時間;實操后才可以用二噴或濕噴。