1、砌體墻無架眼施工
工藝做法:首先在腳手架鋼管橫桿末端焊接一個T型扁鐵,砌筑高度達到搭設點,搭設點應選在豎向灰縫和水平縫的交叉處;搭設腳手架時,橫桿末端的T型扁鐵可以支撐在墻上,放置扁鐵的地方不能放砂漿,方便拆裝。
2、構造柱、圈梁無架眼模板新工藝
流程1:
在“GZ”模板斷面預埋φ14對拉螺栓(外接15PVC塑料管)固定模板,代替砌筑時留的分格孔,提高了墻體的整體砌筑效果。具體施工工藝操作:“GZ”模板采用12mm厚膠合板,與三根50mm×80mm普通木梁連成一體,即“GZ”模板每邊使用一套模板。
Masonry method of inclined roof brick at the top of infilled wall
Technological practice: the top brick used for masonry is cut in advance, so that the upper and lower contact surfaces of the inclined top brick are flat, and the angle with the horizontal plane is 60 degrees when laying obliquely.
Advantages: the upper and lower surfaces are all flat, which ensures that the thickness of horizontal mortar joint of masonry is about 10mm, and avoids the common quality problem of excessive mortar joint thickness. The top brick forms an angle of 60 degrees with the horizontal plane, which makes the masonry more dense and makes the masonry better integrated. It avoids the common quality defects of the joint between the infilled wall and the frame beam after plastering. Convenient construction, neat masonry and good visual quality.
粉刷石膏替代水泥砂漿或混合砂漿在室內抹灰工程中的應用技術
施工做法:抹灰石膏分為底層抹灰石膏和面層抹灰石膏。底層粉刷石膏用于粉刷和找平粉刷墻壁。厚度視基層的平整度和垂直度而定,能蓋住基層即可,薄的部分不小于5 mm,操作方法同水泥砂漿抹灰。也可采用機械攪拌、噴漿和人工刮擦的方法進行找平。面層抹石膏作找平層覆蓋,用鋼抹子刮一薄層,使找平層表面的砂坑填平,表面光滑,厚度約1 ~ 2mm。
優點:水砂砂漿或混合砂漿的抹灰層,施工時容易出現空鼓、裂縫等質量通病,交付后由于水泥引起的收縮變形,抹灰面出現龜紋裂縫。粉刷石膏具有早強、快硬、防火、保溫性強、附著力強、自動調節室內濕度、表面觀感細膩舒適的優良特性。因其微膨脹性和強粘結力,能有效防止抹灰裂縫、起皮、脫落。同時對抹灰基層要求低,不需要在基層表面刷任何界面劑或水泥漿就可以直接抹灰。
這批鋼筋需要進行化學檢驗。
(7)、制作鋼筋料卡:列入加工計劃的配料單,需要為每一根編號的鋼筋制作一張料卡,作為鋼筋加工的依據,并作為鋼筋安裝中區分各工程、構件和各種編號鋼筋的標志。
(8)、鋼筋的表面應潔凈、無損傷,油漬、漆漬和鐵銹應在使用前清除。如發現鋼筋表面氧化皮嚴重,或除銹后鋼筋橫截面有嚴重的凹坑、斑點,應剔除。